Chemical Composition
0.05
%  (maximum)  
0.17 to 0.25
%    
0.3 to 0.5
%    
0.18
%  (maximum)  
95.6 to 97.9
%    (estimate)
0.5 to 1
%    
0.5 to 0.8
%    
0.6 to 1.2
%    
0.02
%  (maximum)  
0.02
%  (maximum)  
0.35
%  (maximum)  
0.03
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data