Chemical Composition
1.1
%  (minimum)  
5 to 7
%    
70 to 77.9
%    (estimate)
16 to 23
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®