Chemical Composition
0.61
%    
1.2
%    
97.2
%    (estimate)
0.9
%    
0.1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
223 to 243
   
 
Other Information
DIN 61CrSiV5; WNr. 1.2243. Soft annealed, max 223 HB (according to DIN 17350 for cold drawn products hardness can be up to 20 HB higher). For chisels, tongs, pliers; screw drivers; shear blades.
KRUPP 2243
 