Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For dies, gages, forming rolls, master hobs, cutters; non-deforming, air hardened.
BALDWIN AH
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For dies, gages, forming rolls, master hobs, cutters; non-deforming, air hardened.
 