Range attributes
1.65
%    
11.5
%    
86.8
%    (estimate)
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Germany
For blanking and forming dies, punches; air hardened, nondeforming.
AMBO CR13MW
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For blanking and forming dies, punches; air hardened, nondeforming.
 
Hyperlink attributes
Integer attributes
ID
64528
232016
 