Range attributes
1.1
%    
0.32
%    
1.1
%    
97.3
%    (estimate)
0.18
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Germany
For oil refinery equipment; creep resistant.
NIT CMA
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For oil refinery equipment; creep resistant.
 