Chemical Composition
0.7 to 1.2
%    
0.12
%  (maximum)  
17 to 19
%    
78.3 to 81.6
%    (estimate)
0.7 to 1.4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
270
MPa    
500 to 700
MPa    
12
% strain    
 
Other Information