Chemical Composition
0.5 to 1
%    
0.12
%  (maximum)  
6 to 8
%    
89.9 to 93
%    (estimate)
0.5 to 1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
220
MPa    
420 to 620
MPa    
20
% strain    
 
Other Information