Chemical Composition
0.12
%  (maximum)  
16 to 18
%    
80.4 to 84
%    (estimate)
1
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
241
MPa    
20 to 100
% strain    
 
Other Information
Annealed: 60,000 TS min; 35,000 YS min; 20 El min; 90 HRB max. Ferritic, magnetic, non-hardenable steel with good corrosion resistance; good for nitration work and nitric acid manufacture.
B&W CROLOY 18 (T/P 430)
 
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®