Chemical Composition
0.42
%    
1.3
%    
95.8
%    (estimate)
0.25
%    
0.25
%    
2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Oil hardening, shock resisting tool steel for moderate hot work; for shear blades, dies, punches, chisels, pneumatic tools. Lower carbon version of AISI S-1.