Chemical Composition
0.6
%    
95.8
%    (estimate)
0.85
%    
0.45
%    
2
%    
0.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Oil hardening shock resisting steel capable of high toughness with moderate wear resistance. For punches, dies, shear blades, stamps, and machinery parts. AISI S-5.