Range attributes
0.75
%    
0.91
%    
95.4
%    (estimate)
0.81
%    
0.4
%    
1.78
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For dies, punches, shear blades, knives, rolls; oil hardened, shock resistant.
BALDWIN NO. 1
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For dies, punches, shear blades, knives, rolls; oil hardened, shock resistant.
 