Range attributes
0.6
%    
0.25
%    
95.9
%    (estimate)
0.8
%    
0.25
%    
2
%    
0.2
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
AISI Type S5 shock resisting tool steel.
AL TECH AL-609
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
AISI Type S5 shock resisting tool steel.
 
Hyperlink attributes
Integer attributes
ID
60487
231893
 
Further Information