Coating (low-dilution weld deposit) alloy; Contains DIAMAX C particles in a multi-component Ni-alloy matrix. Matrix alloying elements include Fe, B and Si. For Plow shares, wear rings, roll reamers and drill stabilizers. 54 HRC.
EUTROLOY 16113
 