Chemical Composition
0.001 to 0.005
%    
0.12 to 0.21
%    
96.6 to 97.6
%    (estimate)
0.45 to 0.7
%    
0.45 to 0.6
%    
1.2 to 1.5
%    
0.2 to 0.35
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
689
MPa    
758 to 931
MPa    
18
% strain    
235 to 293
   
 