Chemical Composition
0.5
%    
98.7
%    (estimate)
0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276 to 414
MPa    
552 to 655
MPa    
18 to 28
% strain    
140 to 180
   
 