Chemical Composition
0.25
%  (maximum)  
99 to 99.3
%    (estimate)
0.7
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207 to 310
MPa    
414 to 517
MPa    
22 to 30
% strain    
115 to 140
   
 
Other Information
Cast: 60,000-75,000 TS; 30,000-45,000 YP; 115-140 HB; 22-30 El. For general and structural applications, gears, housings. Excellent weldability. AISI 1020.
BIRDSBORO-20 CN
 