Chemical Composition
0.001
%    
0.14 to 0.2
%    
0.4 to 0.65
%    
96.1 to 97.6
%    (estimate)
0.6 to 1
%    
0.4 to 0.6
%    
0.7 to 1
%    
0.15 to 0.35
%    
0.03 to 0.08
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
689
MPa    
793 to 1000
MPa    
15 to 100
% strain    
 
Other Information
Quenched and tempered: 115,000-145,000 TS; 100,000 YS min; 15 El min (up to 1.5 in. thick). Good strength, toughness and weldability; for structural applications.