Chemical Composition
Mechanical Properties
200
   
 
Other Information
Flux coated electrode containing hard particles for torch build-up on metals; bonding temperature 1400-1600 F. Matrix 200 HB; particles 89-91 HB; Good abrasion resistance.
XUPER DRIL-TEC 8800
 