Chemical Composition
Mechanical Properties
Other Information
Continuous electrode alloy for maintenance and repair welding, joining, build-up and removal of metal. For all steels, nickel alloys and stainless steel; for mining, crushing, construction, lumber, and cement industries. 62 HRC (typical).
ENDOTEC DO.30
 
Links
Organizations

 



No warranty is given for the accuracy of these data