Continuous electrode alloy for maintenance and repair welding, joining, build-up and removal of metal. For mill wobblers, shovel teeth, crusher rolls, buckets, augers, and hydroelectric turbine runners. As deposited work hardens to HRC 45.
ENDOTEC DO.05
 