Chemical Composition
0.35
%  (maximum)  
0.5
%    
96.7 to 97
%    (estimate)
1.5
%    
0.5
%    
0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
655 to 862
MPa    
827 to 1030
MPa    
9 to 14
% strain    
240 to 310
   
 
Other Information
Cast: 120,000-150,000 TS; 95,000-125,000 YP; 9-14 El; 22-30 RA; 240-310 HB; For general and structural castings, shafts, housings, gears. Tough, shock resistant.