Chemical Composition
49
%    
46 to 49
%    (estimate)
2 to 5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Remanence: 21,500 Gausses. Coercive force 20-60 oersteds. Residual induction 16,000-21,500 Gausses. For magnetic devices, telephone switches. Exhibits square hysteresis loop. Non-directional properties, high curie temperature. Permanent magnet.