Chemical Composition
0.15
%  (maximum)  
11 to 13
%    
63.4 to 70.2
%    (estimate)
17 to 19
%    
0.3 to 0.8
%    
1.5 to 2.5
%    
0.08
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 