Range attributes
418 to 744
   
2.1
%    
12.5
%    
83.6
%    (estimate)
0.32
%    
0.45
%    
1
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Heat treated: 744-418 HB; For high performance blanking and cold forming dies, punches, rolls and gages. High resistance to abrasion. AISI D3.
HURON
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Heat treated: 744-418 HB; For high performance blanking and cold forming dies, punches, rolls and gages. High resistance to abrasion. AISI D3.
 