Chemical Composition
0.13
%  (maximum)  
89 to 91.5
%    (estimate)
0.9
%  (maximum)  
8.4 to 9.6
%    
0.13 to 0.32
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
517
MPa    
22 to 100
% strain    
 
Other Information
Double normalized and tempered: 100,000 TS min; 75,000 YS min; 22 El min. Combination of high strength and resistance to brittle fracture at temperatures down to -320 F.