Chemical Composition
0.06 to 0.12
%    
95 to 96.3
%    (estimate)
0.31 to 0.64
%    
3.18 to 3.82
%    
0.18 to 0.37
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
241
MPa    
30 to 100
% strain    
 
Other Information
Normalized: 65,000 TS min; 35,000 YS min; 30 El min; 90 HRB max. Combination of high strength and resistance to brittle fracture at temperatures down to -150 F.
B&W NICOLOY 3 1/2
 
Links



No warranty is given for the accuracy of these data