Chemical Composition
52
%    
8
%    
36
%    (estimate)
4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
10,000 Br, 2.8 (BH) max. For electromechanical devices, speedometers, recorders, hysteresis motors, digital computers. Precipitation hardening. Permanent magnet. Similar to Vicalloy II.