Chemical Composition
0.25 to 0.45
%    
57.6 to 64.8
%    (estimate)
24 to 26
%    
4.5 to 6
%    
2 to 4
%    
4.5 to 6
%    
Co is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
35 to 37
   
 
Other Information