Chemical Composition
2 to 3
%    
39.5 to 53
%    (estimate)
29 to 35
%    
2.5
%  (maximum)  
1
%  (maximum)  
16 to 19
%    
Co is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information