Chemical Composition
0.7
%    
1
%    
94.7
%    (estimate)
2
%    
1.35
%    
0.3
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1830
MPa    
2020
MPa    
1
% strain    
56 to 59
   
 
Other Information
Heat treated: 293,000 TS; 265,000 YS; 1 El; Usual 56-59 HRC; For dies and punches, blanking and forming dies, gages, shear blades, bending tools, stripper plates, master hubs,air hardening. AISI A6 tool steel, wear resistant.