Chemical Composition
0.55
%    
5
%    
90.7
%    (estimate)
0.3
%    
1.3
%    
0.9
%    
1.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
57 to 60
   
 
Other Information
Usual hardness 57-60 HRC; Punch and die steel for hot and cold work applications, For shear blades, chipper knives, forming dies, forging dies, back up rolls, and plastic molds. AISI A8.
AL TECH A-8
 