Range attributes
0.55
%    
5
%    
90.7
%    (estimate)
0.3
%    
1.3
%    
57 to 60
   
0.9
%    
1.25
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Usual hardness 57-60 HRC; Punch and die steel for hot and cold work applications, For shear blades, chipper knives, forming dies, forging dies, back up rolls, and plastic molds. AISI A8.
AL TECH A-8
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Usual hardness 57-60 HRC; Punch and die steel for hot and cold work applications, For shear blades, chipper knives, forming dies, forging dies, back up rolls, and plastic molds. AISI A8.
 
Hyperlink attributes
Integer attributes
ID
60481
231893
 
Further Information



No warranty is given for the accuracy of these data