Chemical Composition
0.07
%  (maximum)  
14 to 15
%    
2.5 to 4.5
%    
73.9 to 80
%    (estimate)
1
%  (maximum)  
3.5 to 5.5
%    
0.15-0.45 Nb+Ta
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
758
MPa    
1030
MPa    
38
 (maximum)  
 
Other Information
Condition A: 150 ksi TS; 110 ksi YS; 38 max HRC; Precipitation hardening. For high-strength fittings, bolts, shafting, instruments, aerospace hardware.