Range attributes
0.15
%  (maximum)  
24 to 30
% strain    
95.7 to 95.8
%    (estimate)
0.65
%    
3.5
%    
414 to 552
MPa    
276 to 379
MPa    
 
Logical attributes
Yes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Cast: 60,000-80,000 TS; 40,000-55,000 YP; 24-30 El; 35-50 RA. For general and structural castings, gears, housings, shafts. ASTM A352, LC3; AISI 4812 modified. Tough, shock resistant.
BIRDSBORO-LC3
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Cast: 60,000-80,000 TS; 40,000-55,000 YP; 24-30 El; 35-50 RA. For general and structural castings, gears, housings, shafts. ASTM A352, LC3; AISI 4812 modified. Tough, shock resistant.
 