Chemical Composition
0.45
%  (maximum)  
95.3 to 95.7
%    (estimate)
0.8
%    
3.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
655 to 827
MPa    
827 to 1000
MPa    
14 to 20
% strain    
 
Other Information
Heat treated: 120,000-145,000 TS; 95,000-120,000 YP; 14-20 El; 0-40 RA. For general and structural castings, shafts, gears, housings. AISI 2340. Tough, shock resistant.