Chemical Composition
2 to 2.2
%    
97.8 to 98
%    (estimate)
Cu is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
414 to 483
MPa    
586 to 621
MPa    
4 to 12
% strain    
200 to 220
   
 
Other Information
Cast: 85,000-90,000 TS; 60,000-70,000 YS; 4-12 El; 9 RA; 200-220 HB; For gears, shafting welding dies and welding electrodes; corrosion resistant, age hardening.