Chemical Composition
96.2 to 96.6
%    (estimate)
3
%    
0.4 to 0.8
%    
Mg is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
110 to 193
MPa    
207 to 276
MPa    
8 to 10
% strain    
60 to 80
HV    
 