Chemical Composition
0.05 to 0.15
%    
0.003
%    
0.03
%  (maximum)  
8.5 to 9.5
%    
58.1 to 68.3
%    (estimate)
4.6 to 5.2
%    
18 to 19
%    
0.5 to 8
%    
0.02
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
2010
MPa    
2030
MPa    
11.5
% strain    
48 to 50
   
 
Other Information
Maraged: 295,000 TS; 292,000 YS; 11.5 El; 59 RA, 48-50 HRC; For rocket cases, aircraft landing gears, missile and aircraft components. Maraging steel, high strength, ductility and toughness.