Chemical Composition
0.9 to 1.35
%    
0.05
%  (maximum)  
12.3 to 13.3
%    
0.2
%  (maximum)  
2 to 2.5
%    
7.5 to 8.5
%    
0.01
%  (maximum)  
0.008
%  (maximum)  
0.1
%  (maximum)  
 
Mechanical Properties
DimensionsYield Strength (ksi)Ultimate Tensile Strength (ksi)Elongation (% strain)Brinell Hardness
Thickness, 12 in. max≥ 175≥ 185≥ 11≥ 380

175
ksi  (minimum)  
185
ksi  (minimum)  
11
% strain  (minimum)  
380
 (minimum)  
 