Chemical Composition
0.19
%    
0.50
%    
96.2
%    (estimate)
1.20
%    
0.50
%    
1.20
%    
0.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
180
ksi    
15
% strain    
388 to 429
   
 
Other Information
Links
 



No warranty is given for the accuracy of these data