Layout: No layout
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
UK Imperial
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
US Customary
S13800 Type XM-13, ASME SA705/SA705M, Forging; H1000
add data link
Range attributes
Al (Aluminum)
0.9 to 1.35
%
Brinell Hardness
400
(minimum)
C (Carbon)
0.05
% (maximum)
Cr (Chromium)
12.3 to 13.3
%
Elongation
10
% strain (minimum)
Mn (Manganese)
0.2
% (maximum)
Mo (Molybdenum)
2 to 2.5
%
Ni (Nickel)
7.5 to 8.5
%
P (Phosphorus)
0.01
% (maximum)
S (Sulfur)
0.008
% (maximum)
Si (Silicon)
0.1
% (maximum)
Ultimate Tensile Strength
205
ksi (minimum)
Yield Strength
190
ksi (minimum)
Discrete attributes
~Checking Status
Verified - New record
Date Last Checked
Monday, January 8, 2018
Alloy Family
High-Alloy Steel (Corrosion and Heat Resistant, Stainless, and Nickel Steels)
Alloy Group
Precipitation-hardening stainless steel
Alloy Sub-Group
Miscellaneous precipitation-hardening steels
Available forms
Forging
Base Element
Fe (Iron)
Country
USA
Material Class
Ferrous Alloy
Source
BPVC Section II-Materials-Part A-Ferrous Materials Specifications
Specification Status
Active
Specification Type
Standard
Standards Body
ASME (USA)
Short text attributes
Designation
S13800 Type XM-13
Similar UNS Number
S13800
Similar US Grade
S13800
Specification
ASME SA705/SA705M
Long text attributes
Description
Age-hardening stainless steel forgings, Condition H1000
Organization
ASME International (ASME)
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Integer attributes
Specification Year
2011
Tabular attributes
Tabular Data
Hide table
Save as CSV
Copy To Clipboard
Dimensions
Yield Strength (ksi)
Ultimate Tensile Strength (ksi)
Elongation (% strain)
Brinell Hardness
Thickness, 12 in. max
≥ 190
≥ 205
≥ 10
≥ 400
Save as CSV
Copy To Clipboard
Further Information
Organizations
ASME International (ASME)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard