Layout: Organizations Layout
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
Organizations Layout (Default)
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
UK Imperial
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
Metric
SI (Consistent)
US Customary
Eutectic Corp.
add data link
Details
Organization Type
Manufacturer
Active Status
Active
Full Address
Organization Name
Eutectic Corp.
Division
Member of Eutectic + Castolin Companies
Address
9600H Southern Pine Boulevard
City
Charlotte
State
NC
RegionCode
28273
Country
USA
Phone
800 221 1433
Fax
704 527 0812
Links
Materials
Austenitic wrought stainless steel, CEC 57 (Eutectic Corp.)
Austenitic wrought stainless steel, CPW 1933 (Eutectic Corp.)
Austenitic wrought stainless steel, EUTECTRODE 54-L (Eutectic Corp.)
Austenitic wrought stainless steel, EUTECTRODE E308L-16 (Eutectic Corp.)
Austenitic wrought stainless steel, EUTECTRODE E309L-16 (Eutectic Corp.)
Austenitic wrought stainless steel, EUTECTRODE E312-16 (Eutectic Corp.)
Austenitic wrought stainless steel, EUTROLOY 16300LC (Eutectic Corp.)
Austenitic wrought stainless steel, STAINTRODE A (Eutectic Corp.)
Austenitic wrought stainless steel, STAINTRODE A-MO (Eutectic Corp.)
Austenitic wrought stainless steel, STAINTRODE A-MO-L (Eutectic Corp.)
Austenitic wrought stainless steel, STAINTRODE B-L (Eutectic Corp.)
Austenitic wrought stainless steel, STAINTRODE BMO-L (Eutectic Corp.)
Austenitic wrought stainless steel, STAINTRODE D (Eutectic Corp.)
Austenitic wrought stainless steel, TIG-TECTIC D (Eutectic Corp.)
Carbide-base ceramic, EUTECDUR ED-5000 (Eutectic Corp.)
Carbide-base ceramic, EUTECDUR ED-8000 (Eutectic Corp.)
Carbide-base ceramic, GRITALLOY 10011 (Eutectic Corp.)
Carbide-base ceramic, TUNGTEC 10112 (Eutectic Corp.)
Carbide-base ceramic, ULTIMIUM N 112 (Eutectic Corp.)
Carbide-base ceramic, ULTIMIUM N 113 (Eutectic Corp.)
Carbide-base ceramic, ULTIMIUM N 114 EXPRESS (Eutectic Corp.)
Cast high-copper alloy, BRONZOCHROM NO. 185 (Eutectic Corp.)
Cobalt-chromium-tungsten, EUTALLITE-6 (Eutectic Corp.)
Cobalt-chromium-tungsten, EUTECROD 91 (Eutectic Corp.)
Cobalt-chromium-tungsten, EUTROLOY 16001 (Eutectic Corp.)
Cross reference, CASTEC (Eutectic Corp.)
Cross reference, EUTECROD 185 (Eutectic Corp.)
Cross reference, EUTECTRODE 57 (Eutectic Corp.)
Cross reference, EUTECTRODE 240 (Eutectic Corp.)
Cross reference, EUTECTRODE N 2 (Eutectic Corp.)
Cross reference, EUT-O-MAT 3010A (Eutectic Corp.)
Cross reference, EUT-O-MAT 3205 (Eutectic Corp.)
Cross reference, EUT-O-MAT 4601A (Eutectic Corp.)
Cross reference, EUT-O-MAT 4625A (Eutectic Corp.)
Cross reference, EUT-O-MAT AN690 (Eutectic Corp.)
Cross reference, MICROFLO (Eutectic Corp.)
Cross reference, NITECTIC 222 (Eutectic Corp.)
Cross reference, STAINTRODE B (Eutectic Corp.)
Cross reference, STAINTRODE B-MO (Eutectic Corp.)
Cross reference, STEELTECTIC (Eutectic Corp.)
Cross reference, TEROMATEC (Eutectic Corp.)
Cross reference, TIG-TECTIC 2-24 (Eutectic Corp.)
Cross reference, TIG-TECTIC A-MO (Eutectic Corp.)
Cross reference, XUPER 9080 (Eutectic Corp.)
Cross reference, XUPERBOND (Eutectic Corp.)
Cross reference, XYRON 2-23 (Eutectic Corp.)
Cross reference, XYRON 2-24 (Eutectic Corp.)
Martensitic stainless steel, EUTROLOY 16410 (Eutectic Corp.)
Martensitic stainless steel, HARDTEC 19400 (Eutectic Corp.)
Martensitic stainless steel, METACERAM 29012 (Eutectic Corp.)
Molybdenum high-speed tool steel, EUTROLOY 16720 (Eutectic Corp.)
Nickel with chromium and/or iron, molybdenum, CPW 1932 (Eutectic Corp.)
Nickel with chromium and/or iron, molybdenum, EUTROLOY 16494 (Eutectic Corp.)
Nickel with chromium and/or iron, molybdenum, EUTROLOY 16497 (Eutectic Corp.)
Nickel with chromium and/or iron, molybdenum, EUTROLOY 16801 (Eutectic Corp.)
Nickel with chromium and/or iron, molybdenum, EUTROLOY 16802 (Eutectic Corp.)
Nickel with chromium and/or iron, molybdenum, THERMOTEC 18928 (Eutectic Corp.)
Oxide-base ceramic, THERMOTEC 18927 (Eutectic Corp.)
Silver, EUTECROD 1801 (Eutectic Corp.)
Silver, EUTECROD 1810 (Eutectic Corp.)
Silver, EUTECSIL 1801 FC (Eutectic Corp.)
Silver, EUTECSIL 1828 XFC (Eutectic Corp.)
Silver, EUTECSILVERWELD ECON 1 (Eutectic Corp.)
Silver, EUTECSILVERWELD ECON 2 (Eutectic Corp.)
Silver, EUTECUSHION SHIM III (Eutectic Corp.)
Silver, FLOTECTIC SILVER 2 (Eutectic Corp.)
Silver, XUPER 1020 XFC (Eutectic Corp.)
Tin-silver, EUTECROD 157 (Eutectic Corp.)
Unclassified alloy steel, CUT TRODE (Eutectic Corp.)
Unclassified alloy steel, DURFACE (Eutectic Corp.)
Unclassified alloy steel, ENDOTEC DO.29S (Eutectic Corp.)
Unclassified alloy steel, ENDOTEC DO.66 (Eutectic Corp.)
Unclassified alloy steel, EUTROLOY 16550 (Eutectic Corp.)
Unclassified alloy steel, SPRAM 14493 (Eutectic Corp.)
Unclassified carbon steel, BEAUTYWELD (Eutectic Corp.)
Unclassified cast copper, EUTEC ROD 1850FC (Eutectic Corp.)
Unclassified cast iron, CASTEC 3055 (Eutectic Corp.)
Unclassified cast iron, EUTEC ROD 14 (Eutectic Corp.)
Unclassified cast iron, EUTEC TRODE 24/49 (Eutectic Corp.)
Unclassified cast iron, XUPER MODULTEC 2250 (Eutectic Corp.)
Unclassified cast iron, XYRON 2-25 (Eutectic Corp.)
Unclassified cast iron, XYRON 2-26 (Eutectic Corp.)
Unclassified ceramic material, THERMOTEC 18925 (Eutectic Corp.)
Unclassified ceramic material, THERMOTEC 18933 (Eutectic Corp.)
Unclassified cobalt, EUTROLOY 16021 (Eutectic Corp.)
Unclassified cobalt, THERMOTEC 18949 (Eutectic Corp.)
Unclassified high-strength steel, EUTECROD 1600 SUPER (Eutectic Corp.)
Unclassified high-strength steel, OA 690 (Eutectic Corp.)
Unclassified high-strength steel, OA 2020 (Eutectic Corp.)
Unclassified iron alloy, CPW 1930 (Eutectic Corp.)
Unclassified iron alloy, TIG-TECTIC 224 (Eutectic Corp.)
Unclassified iron alloy, XUPER 22-33N (Eutectic Corp.)
Unclassified iron alloy, XUPER 22.40 (Eutectic Corp.)
Unclassified iron alloy, XUPER 2240 (Eutectic Corp.)
Unclassified metal, ABRATEC N700 (Eutectic Corp.)
Unclassified metal, BOROTEC 10009 (Eutectic Corp.)
Unclassified metal, BUILDTEC 25685 (Eutectic Corp.)
Unclassified metal, CHAMFERTRODE (Eutectic Corp.)
Unclassified metal, CHROM-TEC 19222 (Eutectic Corp.)
Unclassified metal, CUTTRODE 1 (Eutectic Corp.)
Unclassified metal, DIAMAX 19112 (Eutectic Corp.)
Unclassified metal, DUROTEC 19910 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.04 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.05 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.10 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.14 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.23 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.29 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.30 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.60 (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.68S (Eutectic Corp.)
Unclassified metal, ENDOTEC DO.80 (Eutectic Corp.)
Unclassified metal, ENDOTEC XO.03 (Eutectic Corp.)
Unclassified metal, EUTALLITE UNIVERSAL 10092 (Eutectic Corp.)
Unclassified metal, EUTECBOR 9000 (Eutectic Corp.)
Unclassified metal, EUTECROD 14 FC (Eutectic Corp.)
Unclassified metal, EUTECROD 15 (Eutectic Corp.)
Unclassified metal, EUTECROD 16 FC (Eutectic Corp.)
Unclassified metal, EUTECROD 18 FC (Eutectic Corp.)
Unclassified metal, EUTECROD 21-FC-E (Eutectic Corp.)
Unclassified metal, EUTECROD 80 FC (Eutectic Corp.)
Unclassified metal, EUTECROD 141 (Eutectic Corp.)
Unclassified metal, EUTECROD 146 FC (Eutectic Corp.)
Unclassified metal, EUTECROD 155 (Eutectic Corp.)
Unclassified metal, EUTECROD 157-B (Eutectic Corp.)
Unclassified metal, EUTECROD 158-B (Eutectic Corp.)
Unclassified metal, EUTECROD 180 (Eutectic Corp.)
Unclassified metal, EUTECROD 185 FC (Eutectic Corp.)
Unclassified metal, EUTECROD 186 FC (Eutectic Corp.)
Unclassified metal, EUTECROD 190 (Eutectic Corp.)
Unclassified metal, EUTECROD 196 (Eutectic Corp.)
Unclassified metal, EUTECROD 800 (Eutectic Corp.)
Unclassified metal, EUTECROD 1601 (Eutectic Corp.)
Unclassified metal, EUTECROD 1702 (Eutectic Corp.)
Unclassified metal, EUTECROD 1803 (Eutectic Corp.)
Unclassified metal, EUTECROD 1804 (Eutectic Corp.)
Unclassified metal, EUTECROD 1900 (Eutectic Corp.)
Unclassified metal, EUTECROD 1909 (Eutectic Corp.)
Unclassified metal, EUTECSIL 1020 FC (Eutectic Corp.)
Unclassified metal, EUTECSIL 1630 FC (Eutectic Corp.)
Unclassified metal, EUTEC-SILWELD 1618 (Eutectic Corp.)
Unclassified metal, EUTEC-TIN-WELD I (Eutectic Corp.)
Unclassified metal, EUTEC-TINWELD II (Eutectic Corp.)
Unclassified metal, EUTEC-TINWELD III (Eutectic Corp.)
Unclassified metal, EUTEC-TINWELD IV (Eutectic Corp.)
Unclassified metal, EUTECTRODE 27 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 40 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 53 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 53-L (Eutectic Corp.)
Unclassified metal, EUTECTRODE 54 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 66 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 71 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 232 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 244 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 280 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 300 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 501 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 518 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 526 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 680 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 691 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 1851 (DC) (Eutectic Corp.)
Unclassified metal, EUTECTRODE 2101 (Eutectic Corp.)
Unclassified metal, EUTECTRODE 6800 (Eutectic Corp.)
Unclassified metal, EUTECTRODE N5005 (Eutectic Corp.)
Unclassified metal, EUTECTRODE N 61 (Eutectic Corp.)
Unclassified metal, EUTECTRODE N 90 (Eutectic Corp.)
Unclassified metal, EUTECTRODE SUPER 110 (Eutectic Corp.)
Unclassified metal, EXOTEC 29904 (Eutectic Corp.)
Unclassified metal, LUBROTEC 19985 (Eutectic Corp.)
Unclassified metal, METACERAM 21021 (Eutectic Corp.)
Unclassified metal, METACERAM 25020 (Eutectic Corp.)
Unclassified metal, METACERAM 25050 (Eutectic Corp.)
Unclassified metal, NEU-TEC-TRONIC 157 BN (Eutectic Corp.)
Unclassified metal, NUCLEOTEC 2222 (Eutectic Corp.)
Unclassified metal, OA 688 (Eutectic Corp.)
Unclassified metal, PROXON 19121 (Eutectic Corp.)
Unclassified metal, PROXON 19132 (Eutectic Corp.)
Unclassified metal, REPAROX XFC (Eutectic Corp.)
Unclassified metal, SPRAM 14112 (Eutectic Corp.)
Unclassified metal, SPRAM 14494 (Eutectic Corp.)
Unclassified metal, SPRAM 14495 (Eutectic Corp.)
Unclassified metal, SPRAM 14496 (Eutectic Corp.)
Unclassified metal, SPRAM 14496 DIAMAX (Eutectic Corp.)
Unclassified metal, TEROCOTE (Eutectic Corp.)
Unclassified metal, TIG-TECTIC 5-AH (Eutectic Corp.)
Unclassified metal, TIG-TECTIC 23 (Eutectic Corp.)
Unclassified metal, TIG-TECTIC 182 (Eutectic Corp.)
Unclassified metal, TIG-TECTIC 183 (Eutectic Corp.)
Unclassified metal, TIG-TECTIC 6800 (Eutectic Corp.)
Unclassified metal, TIN WELD 1 (Eutectic Corp.)
Unclassified metal, TIN WELD 3 (Eutectic Corp.)
Unclassified metal, ULTRALOY 10611 (Eutectic Corp.)
Unclassified metal, VEROTEC 19666 (Eutectic Corp.)
Unclassified metal, XHD 646 (Eutectic Corp.)
Unclassified metal, XHD 2222 (Eutectic Corp.)
Unclassified metal, XHD 6899 (Eutectic Corp.)
Unclassified metal, XHD ABRATEC N6710 (Eutectic Corp.)
Unclassified metal, XHD ABRATEC N6715 (Eutectic Corp.)
Unclassified metal, XHD CASTOSTAR I (Eutectic Corp.)
Unclassified metal, XUPER 18 XFC (Eutectic Corp.)
Unclassified metal, XUPER 146XFC (Eutectic Corp.)
Unclassified metal, XUPER 2100 (Eutectic Corp.)
Unclassified metal, XUPER DIAMAX 10999 (Eutectic Corp.)
Unclassified metal, XUPER DRIL-TEC 8800 (Eutectic Corp.)
Unclassified metal, XUPER ELASTODUR R8811 (Eutectic Corp.)
Unclassified metal, XUPER EUTECBOR 9000 (Eutectic Corp.)
Unclassified metal, XUPER EXOTRODE (Eutectic Corp.)
Unclassified metal, XUPER NUCLEOTEC 2222 (Eutectic Corp.)
Unclassified metal, XUPER ULTRABOND 50000 (Eutectic Corp.)
Unclassified metal, XYRON 244 (Eutectic Corp.)
Unclassified miscellaneous alloy, DRIL-TEC 88 (Eutectic Corp.)
Unclassified miscellaneous alloy, ENTECROD 192 (Eutectic Corp.)
Unclassified miscellaneous alloy, SUPER BRONZOCHROM 10186 (Eutectic Corp.)
Unclassified nickel, BRONZOCHROM 10185 (Eutectic Corp.)
Unclassified nickel, BUILDTEC 10225 (Eutectic Corp.)
Unclassified nickel, CHROMTEC 10680 (Eutectic Corp.)
Unclassified nickel, CPW 1912 (Eutectic Corp.)
Unclassified nickel, EUTEC TRODE 24 (Eutectic Corp.)
Unclassified nickel, EUTROLOY 16113 (Eutectic Corp.)
Unclassified nickel, EUTROLOY 16223 (Eutectic Corp.)
Unclassified nickel, METACERAM 21022 (Eutectic Corp.)
Unclassified nickel, METACERAM 21041 (Eutectic Corp.)
Unclassified nickel, METACERAM 23005 (Eutectic Corp.)
Unclassified nickel, METACERAM 29123 (Eutectic Corp.)
Unclassified nickel, NITEC 10224 (Eutectic Corp.)
Unclassified nickel, STAINTEC 10670 (Eutectic Corp.)
Unclassified nickel, THERMOTEC 18923 (Eutectic Corp.)
Unclassified nickel, THERMOTEC 18930 (Eutectic Corp.)
Unclassified nickel, THERMOTEC 18972 (Eutectic Corp.)
Unclassified nickel, THERMOTEC 18976 (Eutectic Corp.)
Unclassified nickel, THERMOTEC 18990 (Eutectic Corp.)
Unclassified nickel, THERMOTEC 18995 (Eutectic Corp.)
Unclassified nickel, THERMOTEC 18996 (Eutectic Corp.)
Unclassified nickel, TIG-TECTIC 222 (Eutectic Corp.)
Unclassified nickel, TOOLTEC 10675 (Eutectic Corp.)
Unclassified stainless steel, CORORESIST 19300 (Eutectic Corp.)
Unclassified stainless steel, EUTECTRODE 554-L (Eutectic Corp.)
Unclassified stainless steel, EUTECTRODE 670 (Eutectic Corp.)
Unclassified stainless steel, EUTECTRODE E310-16 (Eutectic Corp.)
Unclassified stainless steel, EUTECTRODE E316L-16 (Eutectic Corp.)
Unclassified stainless steel, EUTECTRODE E317L-16 (Eutectic Corp.)
Unclassified stainless steel, EUTECTRODE E347-16 (Eutectic Corp.)
Unclassified stainless steel, STAINTIN 157PA (Eutectic Corp.)
Unclassified stainless steel, TIG-TECTIC A (Eutectic Corp.)
Unclassified stainless steel, TIG-TECTIC AMO-L (Eutectic Corp.)
Unclassified steel, CHROMCARB N-6006 (Eutectic Corp.)
Unclassified steel, DYNATRODE 666 (Eutectic Corp.)
Unclassified steel, DYNATRODE 777 (Eutectic Corp.)
Unclassified steel, EUTECTRODE 65 (Eutectic Corp.)
Unclassified steel, FANTASTEC (Eutectic Corp.)
Unclassified steel, FERROTRODE-2-B (Eutectic Corp.)
Unclassified steel, FERROTRODE 2-B (Eutectic Corp.)
Unclassified steel, OA 3010 (Eutectic Corp.)
Unclassified steel, OA 4601 (Eutectic Corp.)
Unclassified steel, OA 4625 (Eutectic Corp.)
Unclassified steel, OA 4650 (Eutectic Corp.)
Unclassified steel, STEELTECTIC N (Eutectic Corp.)
Unclassified steel, THERMOTEC 18940P (Eutectic Corp.)
Unclassified steel, THERMOTEC 18943 (Eutectic Corp.)
Unclassified steel, TIG-TECTIC 5-HSS (Eutectic Corp.)
Unclassified steel, TIG-TECTIC 5-HW (Eutectic Corp.)
Unclassified steel, TIG-TECTIC 5-OH (Eutectic Corp.)
Unclassified steel, TIG-TECTIC 5-WH (Eutectic Corp.)
Unclassified steel, TIG-TECTIC 66 (Eutectic Corp.)
Unclassified steel, TIG-TECTIC 670 (Eutectic Corp.)
Unclassified steel, TIG-TECTIC 680 (Eutectic Corp.)
Unclassified steel, TIG-TECTIC B (Eutectic Corp.)
Unclassified steel, TOOLTECTIC 6 HSS (Eutectic Corp.)
Unclassified steel, TOOLTECTIC 6 OH (Eutectic Corp.)
Unclassified steel, TOOLTECTIC 6 SH (Eutectic Corp.)
Unclassified steel, TOOLTECTIC 6HW (Eutectic Corp.)
Unclassified steel, TOOLTECTIC 6WH (Eutectic Corp.)
Unclassified steel, TOOLTECTIC 623 (Eutectic Corp.)
Unclassified steel, UNIMATIC 6000 (Eutectic Corp.)
Unclassified steel, XHD 66 (Eutectic Corp.)
Unclassified steel, XHD N102 (Eutectic Corp.)
Unclassified steel, XUPER 16 XFC (Eutectic Corp.)
Unclassified steel, XUPER 680 CGS (Eutectic Corp.)
Unclassified tin, BABTEC 29240 (Eutectic Corp.)
Unclassified tin, CPW 1954 (Eutectic Corp.)
Unclassified tin, CPW 1966 (Eutectic Corp.)
Unclassified wrought aluminum, ALUTEC 29210 (Eutectic Corp.)
Unclassified wrought aluminum, CPW 1961 (Eutectic Corp.)
Unclassified wrought aluminum, CPW 1962 (Eutectic Corp.)
Unclassified wrought aluminum, EUTEC TRODE 2100 (Eutectic Corp.)
Unclassified wrought aluminum, THERMOTEC 18909 (Eutectic Corp.)
Unclassified wrought aluminum, TIG-TECTIC 21 (Eutectic Corp.)
Unclassified wrought aluminum, TIG-TECTIC 21FC (Eutectic Corp.)
Unclassified wrought aluminum, TIG-TECTIC 1851 (Eutectic Corp.)
Unclassified wrought copper, EUTECROD 16 (Eutectic Corp.)
Unclassified wrought copper, EUTECROD 80 (Eutectic Corp.)
Unclassified wrought copper, EUTROLOY 16868 (Eutectic Corp.)
Unclassified wrought copper, THERMOTEC 18993 (Eutectic Corp.)
Unclassified zinc, CORRESIST 29230 (Eutectic Corp.)
Unclassified zinc, CPW 1960 (Eutectic Corp.)
Unclassified zinc, EUTECROD 19 (Eutectic Corp.)
Wrought brass, EUTECROD 18 (Eutectic Corp.)
Wrought bronze, DYNABRAZE 145 FC (Eutectic Corp.)
Wrought bronze, FRIXTEC 19850 (Eutectic Corp.)
Wrought bronze, METACERAM 29061 (Eutectic Corp.)
Wrought bronze, XHD 2800 (Eutectic Corp.)
Wrought bronze, XUPER 146 XFC (Eutectic Corp.)
Wrought bronze, XUPER BRONZTEC 19868 (Eutectic Corp.)
Wrought copper, BRONZOCHROM NO. 186 (Eutectic Corp.)
Wrought copper, BRONZOCHROM NO. 187 (Eutectic Corp.)
Wrought copper, CUPROTEC 10180 (Eutectic Corp.)
Wrought copper, EUTEC ROD 189 (Eutectic Corp.)
Wrought copper, EUTEC ROD 1700 (Eutectic Corp.)
Wrought copper, EUTECROD 1800 (Eutectic Corp.)
Wrought copper, THERMOTEC 18980 (Eutectic Corp.)
Wrought copper-nickel, NITUTEC 10020 (Eutectic Corp.)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard