Chemical Composition
0.35
%    
0.86
%    
0.34
%    
0.81
%    
0.35
%    
0.48
%    
 
Mechanical Properties
209 to 220
ksi    
267 to 276
ksi    
13 to 15
% strain    
560 to 580
   
 
Other Information
Heat treated: 267,000-275,000 TS; 209,000-221,000 YS; 13-15 El; 37-51 RA; 560-580 HB; For chisels, punches, hard tools, furnace bars, dies, shears; non-tempering, water hardened.
BALDWIN NO. 711
 