Chemical Composition
0.05
%    
95.4
%    (estimate)
1.6
%    
0.4
%    
2.2
%    
0.4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
110 to 120
ksi    
 
Other Information