Chemical Composition
0.01
%    
99
%    
1.00
%    
 
Mechanical Properties
359
10^7 dyne/cm^2    
379
10^7 dyne/cm^2    
10
% strain    
 
Other Information
Leaded copper. Extruded and drawn rod, bar. For parts machined from rods, current carrying studs, nuts, bolts, parts for fine machining. Rod hard: 55000 psi TS; 52000 psi YS; 10 EL; 55 HRB; Elec. Conductivity 96% IACS. Free cutting high conductivity.