Chemical Composition
0.2 to 0.6
%    
28 to 32
%    
41.3 to 53.8
%    (estimate)
2
%  (maximum)  
18 to 22
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
245
10^7 dyne/cm^2  (minimum)  
450
10^7 dyne/cm^2  (minimum)  
8
% strain  (minimum)  
 
Other Information