Chemical Composition
0.25 to 0.35
%    
97.9 to 98.2
%    (estimate)
1 to 1.25
%    
0.2 to 0.25
%    
0.3
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
448 to 1260
10^7 dyne/cm^2    
621 to 1450
10^7 dyne/cm^2    
7 to 25
% strain    
196 to 480
   
 
Other Information
Heat treated: 90,000-210,000 TS; 65,000-183,000 YS; 7-25 El; 25-55 RA; 196-480 HB; For power shovels, tractor tread steel, mine car wheels; resists shock and wear; IZ-3-56.
BF-MM
 
Links
Organizations

 



No warranty is given for the accuracy of these data