Steel castings, stainless, precipitation hardening; PH Heat Treatment H1150M
ASME International (ASME)
 
Hyperlink attributes
Integer attributes
Tabular attributes
DimensionsYield Strength (10^7 dyne/cm^2)Ultimate Tensile Strength (10^7 dyne/cm^2)Elongation (% strain)Brinell HardnessRockwell 30-T scaleTreatmentHardness ScaleVickers hardness (HV)
None Specified   ≥ 310    

 