Chemical Composition
0.6 to 0.8
%    
0.015
%  (maximum)  
11.5 to 12.5
%    
74.4 to 77.3
%    (estimate)
0.1
%  (maximum)  
1.85 to 2.15
%    
0.01
%  (maximum)  
8.5 to 9.5
%    
0.01
%  (maximum)  
0.005
%  (maximum)  
0.1
%  (maximum)  
0.28 to 0.37
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1100
10^7 dyne/cm^2  (minimum)  
1200
10^7 dyne/cm^2  (minimum)  
12
% strain  (minimum)  
363
 (maximum)  
 